This study addresses the issues related to the quality of the connection between cast iron liners and inserts in a pressure die-cast automotive engine block, along with the macro and micro wear of the cylinder bearing surface. it was found that the commonly used HPDC high-pressure casting technology of Al-Si alloy engine blocks with cast iron liners, in which the cylinder liner is then recreated, does not ensure their metallic connection. The micro-gap created there becomes thicker as the engine is used, which worsens the conditions for heat dissipation from the sleeve to the block. Locally, on the surface of the cylinder bearing surface, reductions in honing effects and longitudinal cracks were observed. The presented literature mechanism of micro wear of the cylinder bearing surface, dependent on the morphology of graphite segregations, was confirmed. The mechanism of creating micro-breaks in the area of phosphoric eutectic and graphite precipitation occurrence was presented, initiated by the formation of microcracks in the eutectic and delaminations at the eutectic-matrix boundary.
Przejdź do artykułu

Bibliografia


[1] Kim, J.-K., Xavier, F.-A. & Kim, D.-E. (2015). Tribological properties of twin wire arc spray coated aluminum cylinder liner. Materials & Design. 84, 231-237. DOI: 10.1016/j.matdes.2015.06.122.

[2] Longa, W. (1978). Theory of foundry processes. AGH, Wydział Odlewnictwa, Instytut Odlewnictwa. (in Polish).

[3] Pietrowski, S. & Szymczak, T. (2004). Construction of the connection between alfined coating and silumin. Archives of Foundry. 4(14), 393-404. (in Polish).

[4] Pietrowski, S. (2004). Construction of the alfined layer on gray cast iron. Archives of Foundry. 4(11), 95-104. (in Polish).

[5] Pietrowski, S. & Szymczak, T. (2006). The influence of selected technological factors on the structure of the alfined layer on iron alloys. Archives of Foundry. 6(19), 251-266. (in Polish).

[6] Pawlus, P., Michalski, J. & Ochwat, S. (2012). Surface characteristics of cylinder liners intended for pouring using the Alfin method. Pomiary Automatyka Robotyka. 4, 61-65. (in Polish).

[7] Mahle Diesel Symposium, Stuttgart 2005.

[8] Volvo, DAF, MAN, PSA-BMW technical information from Mahle project meetings. Unpublished materials. Krotoszyn 2005-2010. (in Polish).

[9] Gruszka, J. (2011). Global trends in cylinder liners technology. Polskie Towarzystwo Naukowe Silników Spalinowych. 50(3), 1-7.

[10] Kozaczewski, W. (2004). Construction of the piston-cylinder group of combustion engines. Wydawnictwa Komunikacji i Łączności WKŁ. (in Polish).

[11] Podrzucki, Cz. (1991). Cast iron: structure, properties, application. Kraków: Wydaw. ZG STOP.

[12] Çakır, M. & Akcay, İ.H. (2014). Frictional behavior between piston ring and cylinder liner in engine condition with application of reciprocating test. International Journal of Materials Engineering and Technology. 11(1), 57-71.

[13] Shirokov, V.V., Arendar, L.A., Slyn’ko, H.I. & Volchok, I.P. (2003). Influence of phosphide eutectics on the wear resistance of high-strength cast irons. Materials Science. 39(2), 295-298. DOI: 10.1023/B:MASC.0000010284.56057.72.

[14] Uetz, H. (1969). Einfluß der honbearbeitung von zylinderlaufbuchsen auf die innere grenz-schicht und den einlaufverschleiß. Forschungsvereinigung Verbrennungskraftmaschinen. MTZ, 3.

[15] Ronen, A., Etsion, I. & Kligerman, Y. (2001). Friction-reducing surface-texturing in reciprocating automotive components. Tribology Transaction. 44(3), 359-366. DOI: 10.1080/10402000108982468.

[16] Picas, J.A., Forn, A. & Matthäus, G. (2006). HVOF coatings as an alternative to hard chrome for pistons and valves. Wear. 261(5-6), 477-484. DOI: 10.1016/j.wear.2005.12.005.

[17] Skopp, A., Kelling, N., Woydt, M. & Bergrer, L.-M. (2007). Thermally sprayed titanium suboxide coatings for piston ring/cylinder liners under mixed lubrication and dry-running conditions. Wear. 262(9-10), 1061-1070. DOI: 10.1016/j.wear.2006.11.012.

[18] Grabon, W., Pawlus, P., Woś, S., Koszela, W. & Wieczorowski, M. (2016). Effects of honed cylinder liner surface texture on tribological properties of piston ring-liner assembly in short time tests. Tribology International. 113, 137-148. DOI: 10.1016/j.triboint.2016.11.025.

[19] Johansson, S., Nilsson, P.H., Ohlsson, R. & Rosén, B.-G. (2011). Experimental friction evaluation of cylinder liner/piston ring contact. Wear. 271(3-4), 625-633. DOI: 10.1016/j.wear.2010.08.028.

[20] Igartua, A., Nevshupa, R., Fernandez, X., Conte, M., Zabala, R., Bernaola, J., Zabala, P., Luther, R. & Rausch, J. (2011). Alternative eco-friendly lubes for clean two-stroke engines. Tribology International. 44(6), 727-736. DOI: 10.1016/j.triboint.2010.01.019.

[21] BN-78/1372-01. Piston combustion engines. Cylinder liners made of alloy cast iron. General requirements and tests. (in Polish).

[22] Orłowicz, A.W., Mróz, M., Tupaj, M., Trytek, A. (2015). Shaping the microstructure of cast iron automobile cylinder liners aimed at providing high service properties. Archives of Foundry Engineering. 15(2), 79-84. DOI : 10.1515/afe-2015-0043.

[23] Orłowicz, A.W. & Trytek, A. (2003). Effect of rapid solidification on sliding wear of iron castings. Wear. 254(1-2), 154-163. DOI: 10.1016/S0043-1648(02)00301-0.

Przejdź do artykułu

Autorzy i Afiliacje

A. Orłowicz
1
ORCID: ORCID
M. Radoń
1
ORCID: ORCID
M. Lenik
1
ORCID: ORCID
G. Wnuk
1
ORCID: ORCID

  1. Rzeszow University of Technology, Poland

Ta strona wykorzystuje pliki 'cookies'. Więcej informacji