Abstrakt

In this study, to investigate effects of tin addition on the microstructures and corrosion properties, Zn-1Mg-xSn (x = 1.0, 2.0 and 5.0 wt.%) ternary zinc alloys were prepared. The experimental results indicated that the Zn-1Mg-2.0 wt.% Sn alloy has the better mechanical properties compared with pure zinc and Zn-1Mg alloy. The tensile strength of the alloy material is 173.2±3.7 MPa, the yield strength is 120.7±2.4 MPa, the elongation is 5.64±0.08% and the hardness is 76.9±0.8 HV. The average degradation rate of the alloys immersion in SBF solution for 60 days is 0.16±0.03 mm/year, and the Zn-1Mg-2.0 wt.% Sn alloy hemolysis rate is only 0.81±0.02%. It is confirmed that the addition of tin is effective to improve the mechanical properties and degradation of Zn-1Mg alloy. It may be a candidate of the clinical application requirements of the degradable implant materials in orthopedics.
Przejdź do artykułu

Autorzy i Afiliacje

Zhouling Long
1
ORCID: ORCID
Haiyang Lang
2
ORCID: ORCID
Jun Ou
2 3
ORCID: ORCID

  1. Materials Science and Engineering, Guilin University of Technology, China
  2. Guilin University of Technology, College of Materials Science and Engineering / Dental Clinic and Experimental Center of Medical Sciences, 12 Jianganroad, Guilin, 541004, Guilin, China
  3. Guilin Medical University, Experimental Center of Medical Sciences, 26, Huanchen Road Guilin, 541002, Guilin, China

Ta strona wykorzystuje pliki 'cookies'. Więcej informacji