Details

Title

Research on Selected Types of Lustrous Carbon Carriers After the High-Temperature Pyrolysis

Journal title

Archives of Foundry Engineering

Yearbook

2021

Volume

vo. 21

Issue

No 1

Affiliation

Kamińska, J. : Łukasiewicz Research Network – Krakow Institute of Technology, Poland ; Stachowicz, M. : Wroclaw University of Technology, Faculty of Mechanical Engineering, Poland ; Kubecki, M. : Łukasiewicz Research Network – Institute for Ferrous Metallurgy, Gliwice, Poland

Authors

Keywords

foundry ; Green moulding sand ; Lustrous carbon ; Pyrolysis ; Core shooting

Divisions of PAS

Nauki Techniczne

Coverage

56-62

Publisher

The Katowice Branch of the Polish Academy of Sciences

Bibliography

[1] Said, R.M., Kamal, M.R.M., Miswan, N.H. & Ng, S.J. (2018). Optimization of Moulding Composition for Quality Improvement of Sand Casting. Journal of Advanced Manufacturing Technology (JAMT). 12(1), 301-310.
[2] Saikaew, C. & Wiengwiset, S. (2012). Optimization of molding sand composition for quality improvement of iron castings. Applied Clay Science. 67, 26-31. DOI: 10.1016/j.clay.2012.07.005.
[3] Kwaśniewska-Królikowska, D. & Holtzer, M. (2013). Selection criteria of lustrous carbon carriers in the aspect of properties of greensand system. Metalurgija. 52(1), 62-64.
[4] LaFay, V. & Crandell, G. (2009). Three Methods of Reducing Seacoal by Adding Graphite into Greensand Molds. Transactions of the American Foundrymen's Society. 117, 789.
[5] Lewandowski J.L. (2000). Lustrous carbon carrier, Przegląd Odlewnictwa, 10, 384-386. (in Polish)
[6] Lewandowski, J.L. (1998). The effect of coal dust on the toxicity of classic moulding sand. Przegląd Odlewnictwa, 10 322-325. (in Polish)
[7] Jelínek, P. & Beňo, J. (2008). Morphological forms of carbon and their utilizations at formation of iron casting surfaces. Archives of Foundry Engineering. 8(2008), 67-70.
[8] Major-Gabryś, K. (2019). Environmentally Friendly Foundry Molding and Core Sands. Journal of Materials Engineering and Performance. 28(7), 3905-3911. DOI: 10.1007/s11665-019-03947-x.
[9] Holtzer, M. (2012). Technologies of moulding and core sands in the aspect of environmental protection. 3rd Conference Hüttenes-Albertus Poland. 19-40. (in Polish)
[10] Holtzer, M., Bobrowski, A., Grabowska, B., Eichholzb, S., & Hodorc, K. (2010). Investigation of carriers of lustrous carbon at high temperatures by infrared spectroscopy (FTIR). Archives of Foundry Engineering. 10(4), 61-68.
[11] Lewandowski, J.L. (1997). Materials for Foundry Moulds. Kraków: WN Akapit. ISBN: 83-7108-21-2. (in Polish)
[12] Holtzer, M. (2005). Can we eliminate coal dust from classic moulding sands? Przegląd Odlewnictwa. 12, 794-798. (in Polish).
[13] Naro, R.L. (2002). Formation and control of lustrous carbon surface defects in iron and steel castings. Transactions-American Foundrymens Society. 1, 815-834.
[14] Naro, R.L. (2002). An Update on the Formation and Control of Lustrous Carbon Surface Defects in Iron Castings. Ductile Iron News. 3.
[15] Campbell, J., & Naro, R.L. (2010). Lustrous Carbon on Gray Iron (10-136). Transactions of the American Foundrymen's Society, 118, 277.
[16] Jelinek, P., Buchtele, J., Fiala, J. (2004). Lustrous carbon and pyrolysis of carbonaceous additives to bentonite sands, Casting Technology, 66 World Foundry Congress, 455-467.
[17] Engelhardt, T. (2016). Low-emission additives to bentonite-bonded moulding sands. Przegląd Odlewnictwa. 66, 220-223. (in Polish)
[18] Holtzer, M., Żymankowska-Kumon, S., Kubecki, M., & Kwaśniewska-Królikowska, D. (2013). Harmfulness assessment of resins used as lustrous carbon carriers in bentonite moulding sands. Archives of Metallurgy and Materials. 58(3), 817-822. DOI: 10.2478/amm-2013-0078M.
[19] Stefański, Z. (2008). New coal dust substitutes for bentonite moulding sands used in manufacture of castings from malleable iron and aluminium alloys. Transactions of the Foundry Research Institute. 4, 5-18.
[20] Wang, Y., Huang, H., Cannon, F.S., Voigt, R.C., Komarneni, S. & Furness, J.C. (2007). Evaluation of volatile hydrocarbon emission characteristics of carbonaceous additives in green sand foundries. Environmental Science & Technology. 41(8), 2957-2963.
[21] Wang, Y., Cannon, F.S. & Li, X. (2011). Comparative analysis of hazardous air pollutant emissions of casting materials measured in analytical pyrolysis and conventional metal pouring emission tests. Environmental Science & Technology. 45(19), 8529-8535. DOI: 10.1021/es2023048.
[22] Jelinek, P., Buchtele, J., Kriz, V., Nemecek, S., Kriz, A., & Fiala, J. (2002). Morphology and Formation of Pyrolytic Carbon in Moulding Mixtures. Acta Metallurgica Slovaca. 8(4), 415-422.
[23] Michta-Stawiarska, T. (1998). Difficulties in stabilizing the properties of classic molding sands. Krzepnięcie Metali i Stopów. 35, PAN - Oddział Katowice PL. ISSN 0208-9386 (in Polish)
[24] Ji, S., Wan, L., & Fan, Z. (2001). The toxic compounds and leaching characteristics of spent foundry sands. Water, Air, and Soil Pollution. 132(3-4), 347-364, DOI: 10.1023/A:1013207000046.
[25] Orlenius, J. (2008). Factors Related to the Formation of Gas Porosity in Grey Cast Iron: Investigation of Core Gas Evolution and Gas Concentrations in Molten Iron. Research Series from Chalmers University of Technology, ISSN 1653-8891, Licentiate Theses.
[26] Bobrowski, A. & Grabowska, B. (2012). The impact of temperature on furan resin and binders structure. Metallurgy and Foundry Engineering. 38, 73-80.
[27] Poljanšek, I. & Krajnc, M. (2005). Characterization of phenol-formaldehyde prepolymer resins by in line FT-IR spectroscopy. Acta Chimica Slovenica. 52, 238-244.
[28] Bobrowski, A., Drożyński, D., Grabowska, B., Kaczmarska, K., Kurleto-Kozioł, Ż., & Brzeziński, M. (2018). Studies on thermal decomposition of phenol binder using TG/DTG/DTA and FTIR-DRIFTS techniques in temperature range 20–500° C. China Foundry. 15(2), 145-151.
[29] Liu, L., Cao, Y. & Liu, Q. (2015). Kinetics studies and structure characteristics of coal char under pressurized CO2 gasification conditions. Fuel. 146, 103-110.
[30] Sonibare, O.O., Haeger, T., & Foley, S.F. (2010). Structural characterization of Nigerian coals by X-ray diffraction, Raman and FTIR spectroscopy. Energy. 35(12), 5347-5353.
[31] Schwan, J., Ulrich, S., Batori, V., Ehrhardt, H. & Silva, S.R.P. (1996). Raman spectroscopy on amorphous carbon films. Journal of Applied Physics. 80(1), 440-447.

Date

2021.03.05

Type

Article

Identifier

DOI: 10.24425/afe.2021.136078

Source

Archives of Foundry Engineering; 2021; vo. 21; No 1; 56-62
×